NASA’s New 3D-Printed Superalloy Can Take the Heat

NASA’s New 3D-Printed Superalloy Can Take the Heat

NASA has demonstrated a breakthrough in 3D printable high-temperature materials that could lead to stronger, more durable parts for airplanes and spacecraft.

A team of innovators from NASA and The Ohio State University detailed the characteristics of the new alloy, GRX-810, in a peer-reviewed paper (SEE BELOW) published in the journal Nature.Ohio State Buckeyes | Ohio State University Athletics

“This superalloy has the potential to dramatically improve the strength and toughness of components and parts used in aviation and space exploration,” said Dr. Tim Smith of NASA’s Glenn Research Center in Cleveland, lead author of the Nature paper. Smith and his Glenn colleague Christopher Kantzos invented GRX-810. 

Smith and his team employed time-saving computer modeling, as well as a laser 3D printing process that fused metals together, layer-by-layer, to create the new alloy. They used this process to produce the NASA logo pictured above.

GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.

Current state-of-the-art 3D printed superalloys can withstand temperatures up to 2,000 degrees Fahrenheit. Compared to those, GRX-810 is twice as strong, over 1,000 times more durable, and twice as resistant to oxidation.

“This new alloy is a major achievement,” said Dale Hopkins, deputy project manager of NASA’s Transformational Tools and Technologies project. “In the very near future, it may well be one of the most successful technology patents NASA Glenn has ever produced.”

A team of contributors from Glenn, NASA’s Ames Research Center in California’s Silicon Valley, NASA’s Marshall Space Flight Center in Huntsville, Alabama, and The Ohio State University co-authored the Nature paper.  

GRX-810 was developed under NASA’s Transformational Tools and Technologies project, with support from the agency’s Game Changing Development Program.

Brian Newbacher
NASA’s Glenn Research Center

Image credit: NASA/ Jordan Salkin

Last Updated: Apr 21, 2023

Editor: Nikki Welch-bey
 
Content Source: NASA
 
A 3D printable alloy designed for extreme environments
 

RELATED CONTENT:

Fastener Design Course by NASA

Enduralock Revolutionary Fastener Technology Wins NASA iTech Competition

 
3D Printing / Additive Manufacturing, 3DP & Additive MFG, Featured

IN THE NEWS – Weekly Fastener News Podcast

Your Digital Ad Space!

Subscribe Today!

Your Digital Ad Space!

Producer Price Index

Goodbye Filtered Search

Your Digital Ad Space!

Fully Threaded Radio

Loading RSS Feed

Your Digital Ad Space!

Fastener TV

Know whats going, now! Join our community and receive updates by email.

Know whats going, now! Join our community and receive updates by email.

Sign up for our mailing list to receive the latest news and updates from Fastener News Desk.

You have Successfully Subscribed!